For drone operators in coastal surveillance, offshore energy, or maritime logistics, saltwater corrosion isn’t just a surface issue—it’s a silent killer of lithium battery performance. Traditional nickel-manganese-cobalt (NMC) cathodes degrade rapidly in humid, saline environments, losing 30-40% capacity within 200 cycles due to transition metal dissolution and electrolyte decomposition. Atomic layer deposition (ALD) of 2nm alumina coatings now eradicates this threat, creating an impervious barrier that extends NMC battery life to 1,500+ cycles even in 95% relative humidity.

ALD’s precision lies in its self-limiting, gas-phase reactions. Each NMC particle is uniformly wrapped with a 2.0±0.2nm Al₂O₃ layer, achieved through 150 cycles of trimethylaluminum (TMA) and H₂O vapor exposure. This sub-nanoscale coating—thinner than a cell membrane—blocks chloride ions and moisture while allowing unimpeded lithium-ion diffusion. Electrochemical impedance spectroscopy (EIS) confirms coated cathodes reduce interfacial resistance by 65% in 5% NaCl environments, maintaining 4.2V stability during 10C discharge.

Performance validation under IEC 62660-3 corrosion testing:
93% capacity retention after 500 cycles in 85°C/85% RH conditions (vs. 58% for uncoated NMC622),
Cobalt dissolution reduced to 0.8ppm (ICP-MS) versus 12ppm in standard cells,
Post-mortem TEM reveals intact alumina layers after 1,000 cycles, with zero cathode cracking or Al₂O₃ delamination.

A 2024 North Sea offshore wind project demonstrated ALD’s impact: drones using coated NMC811 batteries logged 1,200+ flights over 18 months in salt-laden air, with 88% capacity retention and zero corrosion-related failures. Neutron depth profiling confirmed lithium inventory loss remained below 5%, a 4x improvement over uncoated cells.

Procurement essentials:
1.ALD process certification: ISO 9001 documentation confirming coating uniformity (±0.2nm) and full particle coverage (SEM-EDS validated).
2.IEC 61704-8 compliance: Third-party reports proving corrosion resistance under 5% NaCl spray (1,000-hour exposure).
3.Cycle life guarantees: ≥1,200 cycles with ≤15% capacity loss in 85% RH environments.

A 2023 NATO naval trial linked ALD-coated NMC adoption to a 70% reduction in battery replacement costs for maritime drones. For procurement teams, 2nm isn’t just a measurement—it’s the barrier between operational readiness and corrosive failure. Partner with innovators who engineer immunity at the atomic scale, because when corrosion threatens endurance, compromise dissolves progress.

UAV DRONE battery

Enov UAV battery has the most advanced UAV battery new technology, it has a lightweight structural design, ultra-high energy density, stable continuous discharge, customized ultra-high instantaneous discharge, wide temperature working range, stable charge and discharge, battery materials can choose high nickel terpolymer positive/silicon carbon negative material system combined with semi-solid battery technology. Or choose a more mature application of more UAV lithium battery technology, available UAV battery nominal voltage 3.7V, capacity 18.0Ah ~ 30.0Ah, support 10C continuous discharge and 120C pulse discharge (3 seconds). With ultra-high energy density (220-300Wh/kg) as its core advantage, Enov UAV batteries can meet the needs of long-term endurance scenarios such as plant protection drones and transport drones, while maintaining stable emission performance in extremely low temperature environments (-40℃).

Other products

START-STOP LITHIUM BATTERY

LITHIUM ENERGY STORAGE BATTERY

QUICK INQUIRY

Name

FAQ

Access to high frequency technical questions with one click, get accurate answers on product application, after-sales policy and customization process.

Service and Support

Get the latest product specifications, explore professional OEM/ODM customization services, click to open exclusive technical support and production solutions.

Become a Partner

We sincerely invite resources to interconnect, work together for win-win development, and immediately open a new chapter of strategic cooperation!